20 YEARS OF PROFESSIONAL & DEDICATED SERVICE TO GLOBAL CUSTOMERS

Custom Manufacturing, Project Outsourcing, your Trusted Partner from China

Troubleshooting Common AKD Sizing Issues for Paper Manufacturers

Alkyl Ketene Dimer (AKD) wax is a highly effective sizing agent for modern papermaking, offering superior water resistance and enhanced paper properties. However, like any chemical process, achieving optimal results with AKD can sometimes involve overcoming specific challenges. As a dedicated manufacturer and supplier of AKD wax, we are committed to helping paper mills achieve seamless integration and consistent performance. This article addresses common issues encountered with AKD sizing and provides practical troubleshooting solutions.

Common Challenges in AKD Sizing:

  1. Inadequate Sizing (Low Water Resistance): This is perhaps the most frequent issue, manifesting as poor performance in water resistance tests or increased ink feathering.
    • Potential Causes: Insufficient AKD dosage, poor retention of AKD on fibers, incomplete curing (esterification), incorrect pH, or unstable AKD emulsion.
    • Troubleshooting:
      • Verify Dosage: Ensure the AKD dosage aligns with the required sizing level and paper grade.
      • Optimize Retention: Review the use and dosage of retention aids, which are crucial for anchoring AKD to fibers.
      • Check Curing Conditions: The esterification reaction requires adequate heat. Ensure sufficient drying temperature and time in the paper machine’s drying section.
      • Monitor pH: Confirm the process pH is within the optimal range for AKD (neutral to slightly alkaline).
      • Emulsion Stability: An unstable emulsion can lead to uneven application, impacting sizing.
  2. Poor AKD Emulsion Stability: An unstable emulsion can lead to streaky sizing, deposits on machinery, and reduced efficiency.
    • Potential Causes: Improper preparation of the AKD emulsion, incorrect emulsifier selection or dosage, contamination, or improper storage conditions.
    • Troubleshooting:
      • Review Emulsification Process: Ensure correct temperatures, mixing speeds, and reagent addition sequences are followed during emulsion preparation.
      • Select Appropriate Emulsifiers: Work with your supplier to ensure you are using compatible and effective emulsifying agents tailored for AKD.
      • Check Storage: Store AKD and its emulsions under recommended conditions to maintain stability.
  3. Deposits on Paper Machine Equipment: Unreacted AKD or unstable emulsion components can adhere to machine parts, causing operational issues and impacting paper quality.
    • Potential Causes: Over-dosage of AKD, poor emulsion stability, or interactions with other chemicals in the system.
    • Troubleshooting:
      • Optimize Dosage: Reduce AKD dosage if it’s found to be excessive.
      • Improve Emulsion Stability: Address issues contributing to emulsion instability.
      • Chemical Compatibility: Review the compatibility of AKD with all other chemicals in the wet end.
      • Regular Cleaning: Implement a consistent cleaning schedule for machine components.
  4. Variability in Paper Quality: Inconsistent sizing or strength can occur due to fluctuations in the papermaking process.
    • Potential Causes: Variations in AKD dosage, inconsistent pulp properties, or fluctuating machine operating conditions (pH, temperature).
    • Troubleshooting:
      • Standardize Application: Implement strict controls on AKD dosing and application procedures.
      • Monitor Pulp: Ensure consistent pulp quality and preparation.
      • Process Control: Maintain stable machine conditions, especially pH and drying temperatures.
  5. Foaming Issues: While less common with AKD, certain emulsifiers or process conditions can sometimes lead to foaming.
    • Troubleshooting: Adjust AKD and emulsifier levels, or consider using a suitable defoamer.

Our Commitment as Your AKD Wax Supplier

As a dedicated manufacturer and supplier, we aim to provide not only high-quality AKD wax but also the technical expertise to help you overcome any operational challenges. We encourage you to buy AKD wax from us for consistent product performance and reliable support. By understanding these common issues and proactively implementing the troubleshooting steps, paper manufacturers can ensure the efficient and effective use of AKD wax, leading to superior paper quality and production efficiency. Don’t hesitate to contact our technical team for personalized assistance with your AKD sizing process.

Manufacturing Facilities

NINGBO INNO PHARMCHEM CO.,LTD. was established in 2007. It is committed to the R&D, production and sales of raw materials, pharmaceutical intermediates and fine chemicals. We striving to create a high-efficiency and high-quality integrated chemical service platform to better serve domestic and foreign customers.

Professional Export Experience

to Global Customers

WHY CHOSE US?

1. 20 years of R&D, manufacturing and sales experience, serving customers in 60 countries and regions around the world;

2. Own R&D laboratory, pilot platform and large-scale production workshop, which can meet the audit requirements of global customers;

3. We can satisfy customers' perfect transition from small scale lab requirements (gram level) to commercialization requirements (hundred tons level).

FAQ

  • A: We don't have Minimum Order Quantity, exact quantity should be provided before quotation for us to calculate the exact cost.

  • A: We don't provide free samples due to lots of request and expensive international courier's cost, we can deduct the sample charge after commercial order placed.

  • A: Our payment terms: Small or sample order: T/T IN ADVANCE. Commercial order: First order should be by T/T IN ADVANCE or L/C at sight, and following orders T/T 30~90days is acceptable subject to approval of credit application.

CONTACT US
Should you need to contact us; you may call during regular business hours, Monday through Friday, 8am – 6 pm.
NINGBO INNO PHARMCHEM CO.,LTD.
Address: No.163 Ruiqing Rd.,Ningbo 315000 China
Phone: 86-574-87319282
Fax: 86-574-27912196
SEND US AN EMAIL

NAME*

EMAIL*

COMPANY

COUNTRY*

MESSAGE*

Previous: Maximizing Value: Buying AKD Wax at Competitive Prices

Next: Silica Sol in CMP: Achieving Ultra-Smooth Surfaces in Electronics

All Rights Reserved